Hiya guys,
I'm a bit peeved off, got my car resprayed around the 9 years ago, got the car sandblasted, after lets say 3 years, the paint started to bubble. I thought..."humidity bubbles", yeah it happens.....so I didn't think twice about it. The time is now and I've got panels covered in all these "little bubbles", so on further inspection to find out that its actually rust. Not happy Jan! Long story cut short, cheap sand was used to blast the car (sand containing salt), causing what we have to date.
So, my question is
-Re-blast the panels?
-Strip the panels back by hand and deox?
-Should I go soda blasting? Will it removed the impregnated rust?
-Will any of the above guarantee the removal of the rust to never have this problem again?
I'm no panel beater by any means although this is going to be a learning curve for me.
Any one who has had an experience similar to me, I'm all ears!
Would love to know how you've gone about it,
Or if your a panel beater/spray painter, by all means, speak up!
Cheers!